| ▶ 화재 |
| 2010 FTP Code ANNEX 1 Part 5 |
Test for surface flammability(test for surface materials and primary deck coverings) |
CFE : (0.0 ~ 50.5) kW/㎡ |
소재지 |
| ASTM D 2863 - 23 |
Standard Test Method for Measuring the Minimum Oxygen Concentration to Support Candle-Like Combustion of Plastics(Oxygen Index) |
OI : (0.0 ~ 100.0) % |
소재지 |
| ASTM D 3675 - 22 |
Standard Test Method for Surface Flammability of Flexible Cellular Materials Using a Radiant Heat Energy Source |
Is : (0 ~ 1 000) |
소재지 |
| ASTM E 162 - 22 |
Standard Test Method for Surface Flammability of Materials Using a Radiant Heat Energy Source |
Is : (0 ~ 1 000) |
소재지 |
| ASTM E 662 - 21ae1 |
Standard Test Method for Specific Optical Density of Smoke Generated by Solid Materials |
Ds : (0.0 ~ 1 000) |
소재지 |
| ASTM E1354 - 23 |
Standard Test Method for Heat and Visible Smoke Release Rates for Materials and Products Using an Oxygen Consumption Calorimeter |
HRR : (0 ~ 1 000) kW/㎡ THR : (0 ~ 500) MJ/㎡ |
소재지 |
| ASTM E648 - 19ae1 |
Standard Test Method for Critical Radiant Flux of Floor-Covering Systems Using a Radiant Heat Energy Source |
CHF: (1.1 ~ 10.9) kW/㎡ |
소재지 |
| ASTM E970 - 17e1 |
Standard Test Method for Critical Radiant Flux of Exposed Attic Floor Insulation Using a Radiant Heat Energy Source |
CHF: (1.1 ~ 10.9) kW/㎡ |
소재지 |
| BS 6401 : 1983 |
Method for Measurement, in the laboratory, of the specific optical density of smoke generated by materials |
Ds : (0.0 ~ 1 000) |
소재지 |
| BS EN ISO 1182 : 2020 |
Reaction to fire tests for products - Non-combustibility test(ISO 1182:2020) |
△T : (0.0 ~ 500.0) ℃ MLR : (0.0 ~ 100.0) % |
소재지 |
| BS EN ISO 4589-2 : 2017 |
Plastics - Determination of burning behaviour by oxygen index - Part 2: Ambient-temperature test |
OI : (0.0 ~ 100.0) % |
소재지 |
| BS EN ISO 4589-3 : 2017 |
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test |
OI : (0.0 ~ 100.0) % |
소재지 |
| BS EN ISO 5659-2 : 2017 |
Plastics - Smoke generation - Part 2: Determination of optical density by a single-chamber test(ISO 5659-2:2017) |
Ds : (0.0 ~ 1 000) |
소재지 |
| BS EN ISO 9239-1 : 2010 |
Reaction to fire tests for floorings Part 1: Determination of the burning behaviour using a radiant heat source(ISO 9239-1:2010) |
CHF : (1.1 ~ 10.9) kW/㎡ |
소재지 |
| BS ISO 5660-1 : 2015 + A1 : 2019 |
Reaction to fire tests - Heat release, smoke production and mass loss rate - Part 1 : Heat release rate(cone calorimeter method) and smoke production rate(dynamic measurement) |
HRR : (0 ~ 1 000) kW/㎡ THR : (0 ~ 500) MJ/㎡ |
소재지 |
| EN ISO 1182 : 2010 |
Reaction to fire tests for products - Non-combustibility test(ISO 1182:2010) |
△T : (0.0 ~ 500.0) ℃ MLR : (0.0 ~ 100.0) % |
소재지 |
| EN ISO 4589-2 : 2017 |
Plastics - Determination of burning behaviour by oxygen index - Part 2: Ambient-temperature test |
OI : (0.0 ~ 100.0) % |
소재지 |
| EN ISO 4589-3 : 2017 |
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test |
OI : (0.0 ~ 100.0) % |
소재지 |
| EN ISO 5659-2 : 2017 |
Plastics - Smoke generation - Part 2: Determination of optical density by a single-chamber test |
Ds : (0.0 ~ 1 000) |
소재지 |
| EN ISO 9239-1 : 2010 |
Reaction to fire tests for floorings Part 1: Determination of the burning behaviour using a radiant heat source(ISO 9239-1:2010) |
CHF : (1.1 ~ 10.9) kW/㎡ |
소재지 |
| ISO 1182 : 2020 |
Reaction to fire tests for products - Non-combustibility test |
△T : (0.0 ~ 500.0) ℃ MLR : (0.0 ~ 100.0) % |
소재지 |
| ISO 4589-2 : 2017 |
Plastics - Determination of burning behaviour by oxygen index - Part 2: Ambient-tempreature test |
OI : (0.0 ~ 100.0) % |
소재지 |
| ISO 4589-3 : 2017 |
Plastics - Determination of burning behaviour by oxygen index - Part 3: Elevated-temperature test |
OI : (0.0 ~ 100.0) % |
소재지 |
| ISO 5658-2 : 2006 |
Reaction to fire tests- Spread of flame - Part2: Lateral spread on building and transport products in vertical configuration |
CFE : (0.0 ~ 50.5) kW/㎡ |
소재지 |
| ISO 5659-2 : 2017 |
Plastics - Smoke generation-Part 2: Determination of optical density by a single-chamber test |
Ds : (0.0 ~ 1 000) |
소재지 |
| ISO 5660-1 : 2015/Amd 1 : 2019 |
Reaction to fire tests - Heat release, smoke production and mass loss rate - Part 1: Heat release rate(cone calorimeter method) and smoke production rate(dynamic measurement) AMENDMENT 1 |
HRR : (0 ~ 1 000) kW/㎡ THR : (0 ~ 500) MJ/㎡ |
소재지 |
| ISO 9239-1 : 2010 |
Reaction to fire tests for floorings - Part 1: Determination of the burning behaviour using a radiant heat source |
CHF: (1.1 ~ 10.9) kW/㎡ |
소재지 |
| KS F ISO 1182 : 2020 |
화재연소 시험방법-불연성시험 |
△T : (0.0 ~ 500) ℃ MLR : (0.0 ~ 100) % |
소재지 |
| KS F ISO 5660-1 : 2015 |
연소성능시험-열방출률,연기발생률,질량감소율-제1부:열방출률(콘칼로리미터법) 및 연기발생률(동적 측정) |
HRR : (0 ~ 1 000) kW/㎡ THR : (0 ~ 500) MJ/㎡ |
소재지 |
| KS F ISO 9239-1 : 2010 |
바닥재의 화재 시험방법 - 제1부:복사열원을 이용한 연소거동 측정 |
CHF: (1.1 ~ 10.9) kW/㎡ |
소재지 |
| KS M ISO 4589-2 : 2017 |
플라스틱-산소 지수에 의한 연소 거동의 측정-제2부 : 상온시험법 |
OI : (0.0 ~ 100.0) % |
소재지 |
| KS M ISO 4589-3 : 2017 |
플라스틱-산소 지수에 의한 연소 거동의 측정-제3부 : 고온시험법 |
OI : (0.0 ~ 100.0) % |
소재지 |
| KS M ISO 5659-2 : 2017 |
플라스틱-연기발생-제2부:단일 연소 챔버 시험에 의한 광학 밀도 측정 |
Ds : (0.0 ~ 1 000) |
소재지 |